热塑性聚氨酯弹性体(聚酯) TPU BASF Polyurethanes GmbH Elastollan C 80 A材料说明 Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties. Outstanding tensile strength and high elongation at break, good damping characteristics, a high resilience performance and very good wear resistance.

Typical applicationsSpiral tubing, pneumatic tubing, round belting, technical mouldings e.g. bushes, dust caps, seals, joints, blow moulded bellows, fan belts.

下载Elastollan C 80 A物性表

 Elastollan C 80 A物性表基本信息特性 高拉伸强度耐磨损性良好延高的拉伸率有弹性用途 衬套传送带修补管件护罩密封件加工方法 吹塑成型挤出注射成型物理性能额定值单位制测试方法密度 1.19g/cm³ISO 1183/A 硬度额定值单位制测试方法肖氏硬度 (邵氏 A, 3 秒)82ISO 7619 机械性能额定值单位制测试方法磨损量 30.0mm³ISO 4649-A 弹性体额定值单位制测试方法拉伸应力 DIN 53504     20%应变 2.50MPaDIN 53504     100%应变 4.50MPaDIN 53504     300%应变 8.50MPaDIN 53504 拉伸应力 DIN 53504     屈服 135.0MPaDIN 53504     屈服 50.0MPaDIN 53504 伸长率 2(断裂)650%DIN 53504 撕裂强度 365kN/mISO 34-1 压缩永久变形 ISO 815     23°C, 72 hr 25%ISO 815     70°C, 24 hr 35%ISO 815 冲击性能额定值单位制测试方法简支梁缺口冲击强度 ISO 179     -30°C 无断裂ISO 179     23°C 无断裂ISO 179 注射额定值单位制加工(熔体)温度 170 到 240°C 模具温度 20.0 到 70.0°C 挤出额定值单位制熔体温度 150 到 230°C 备注1 .after storage in water for 21 days at 80°C2 .after storage in water for 21 days at 80°C3 .B 方法,直角形试样(割口)

关于Elastollan C 80 A物性表中数据准确性声明

此Elastollan C 80 A物性表中数据由 乐睿 从该原料的生产商处获得。乐睿 尽最大努力确保此物性表的准确性。 但是 乐睿 对Elastollan C 80 A数据值不承担任何责任,并强烈建议在最终选择TPU C80A材料前,就数据值与材料供应商进行验证。

乐睿塑料为您提供详细的Elastollan C 80 A物性表参数。

想了解更多的与Elastollan C 80 A相关的物性参数,请点击 Elastollan TPU树脂 。

如果您对我们的TPU C80A有任何疑问,或者想索取C80A 物性表datasheet、物质安全资料证书MSDS、ROHS检验报告、SGS报告、REACH环保证明、FDA证明、EU法规证明、UL证书及出厂证明COC/COA报告等,敬请拨打我们联系。